Rod seal RSD 24x32x5,8 PU
| Code | RSD 0240 0320 058 C0 | |
|---|---|---|
| Availability | On request |
Technical data
| Seal type | RSD | |
|---|---|---|
| Material type | PU | |
| Material code | C0 | |
| Foreign code | 2ERSD133 | |
| Brand | Artic seals | |
| Weight | 2 | g |
| Rod diameter d | 24 | mm |
|---|---|---|
| Groove Diameter D | 32 | mm |
| Seal width h | 5,8 | mm |
Documents
- Artic RSD - cataloguepdf fileDownload
Description
Rod seal RSD 24x32x5,8 PU [2ERSD133] is a double-lip sealing ring made of polyurethane C0 by the renowned Italian manufacturer Artic Seals. It is designed for use in hydraulic cylinders, where both lips are pressed against the mating surface thanks to the elasticity of the material. The additional lip stabilises the seal and protects it against external contamination. The design of the ring prevents the stick-slip effect and supports sealing performance at low temperatures. The technical data of rod sealnia U RSD 24x32x5,8 PU [2ERSD133] are: Working pressure: up to 400 bar Linear speed: up to 0,5 m/s Hardness: 93 Shore A ±2 Material: polyurethane C0 with high abrasion resistance and low compression set Rod seal RSD 24x32x5,8 PU [2ERSD133] is a high-specification product that will meet the expectations of even the most demanding customers.
Material
PU / TPU / H-PU (polyurethane)
- Standard PU / TPU-30 °C to +80 °C
Best for high pressure and abrasion, in mineral hydraulic oil. Standard PU must never meet hot water, steam or brake fluid, or run hotter than +90 °C.
| Can be used | Do not use |
|---|---|
| Extreme pressure and pulsation (up to 40-50 MPa, very resistant to extrusion into the gap) | Hot water and steam with standard PU: hydrolysis, it breaks down into powder |
| Abrasion, friction, cutting and tearing (4-5 times tougher than NBR) | Glycol brake fluid (DOT 3, DOT 4, DOT 5.1): swells quickly |
| Mineral hydraulic oil (HL, HLP) and grease | High temperatures above +90 to +100 °C with standard TPU: it softens |
| Fuel oil, diesel and technical oils (aliphatic hydrocarbons) | Strong (concentrated) acids and alkalis: sulfuric, nitric, caustic soda |
| Ozone, weather and sunlight (does not crack from weather) | Acetone, MEK, toluene, benzene, dichloromethane (polar and aromatic solvents) |
| Water-based fire-resistant fluids HFA, HFB (only special H-PU) | Synthetic ester oils and fire-resistant fluid HFD-R |
| Dry compressed air and technical gases | Strong alcohols (methanol, ethanol): swelling |
Water and heat destroy standard PU: above +50 to +60 °C in water or damp oil it turns into a sticky paste or crumbles. If the system contains water or an emulsion, use only H-PU (hydrolysis-resistant).